Name | Nickel Iron Alloy |
---|---|
Composition | Ni: 42%, Fe: Balance |
Density | 8.2 G/cm³ |
Thermal Expansion | 1.5 X 10^-6 /°C |
Yield Strength | 600 MPa |
Density | ~8.0 G/cm³ |
---|---|
Tensile Strength | ~690 MPa (100 Ksi) |
Yield Strength | ~400 MPa (58 Ksi) |
Elongation | ~30% |
Machinability | Good |
Composition | Ni: 40%, Fe: Balance |
---|---|
Density | 8.2 G/cm³ |
Thermal Expansion | 1.4 X 10^-6 /°C |
Yield Strength | 600 MPa |
Tensile Strength | 800 MPa |
Density | 8.5g/cm5 |
---|---|
Thermal Conductivity | ~13 W/(m·K) (approximate) |
Yield Strength | ~550 MPa (approximate) |
Elongation | ~20% (approximate) |
Hardness | ~190 HB (Brinell) |
Density | 8.44g/cm3 |
---|---|
Price Term | Discuss |
Alloy Type | Monel Nickel Copper Alloy |
Surface | Black Or Bright |
Product Type | Round Bars, Square Bars, Pipes, Plates, Etc |
Density | 8.1 G/cm³ |
---|---|
Alloy Type | Nickel-based Alloys |
Melting Point | 1320°C-1390°C |
Thermal Expansion Coefficient | 13.5×10-6 M/mK |
Thermal Coefficient | 11 W/(m·K) |
Name | High Performance Nickel Copper Alloy |
---|---|
Chemical Composition | Ni: 63%, Cu: 31%, Fe: ≤2.5%, Mn: ≤1.5%, Ti: 0.35-0.85%, C: ≤0.3% |
Density | 8.44 G/cm³ |
Tensile Strength | Approx. 760 MPa (110 Ksi) |
Yield Strength | Approx. 310 MPa (45 Ksi) |
Name | Nickel Copper Alloy |
---|---|
Chemical Composition | Ni: 63%, Cu: 31%, Fe: ≤2.5%, Mn: ≤1.5%, Ti: 0.35-0.85%, C: ≤0.3% |
Density | 8.44 G/cm³ |
Tensile Strength | Approx. 760 MPa (110 Ksi) |
Yield Strength | Approx. 310 MPa (45 Ksi) |
Name | Nickel Based Alloys |
---|---|
Alloy Type | Nickel-Chromium Superalloy |
Density | ~8.42 G/cm³ (0.305 Lb/in³) |
Melting Point | ~1360-1410°C (2480-2570°F) |
Tensile Strength | ~1100 MPa (160 Ksi) |
Name | Nickel Molybdenum Alloy |
---|---|
Density | ~8.89 G/cm³ (0.320 Lb/in³) |
Melting Point | ~1350-1450°C (2460-2640°F) |
Tensile Strength | ~550 MPa (80 Ksi) |
Yield Strength | ~350 MPa (50 Ksi) |