Gh3039 High Strength Corrosion Resistant Nickel-Based Superalloy For Demanding High-Temperature Applications

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH3039 alloy
Composition:
Nickel-based Superalloy Containing Chromium, Cobalt, Iron, And Other Elements
Density:
8.23 G/cm³
Melting Point:
1320-1370°C (2408-2498°F)
Tensile Strength:
850-1100 MPa (at Room Temperature)
Yield Strength (0.2% Offset):
450-700 MPa
Elongation:
30-50%
Thermal Conductivity:
9.8 W/m·K (at 100°C)
Specific Heat Capacity:
Specific Heat Capacity
Coefficient Of Thermal Expansion:
13.6 µm/m·K (20-100°C)
Electrical Resistivity:
1.10 µΩ·m (at 20°C)
Magnetic Properties:
Non-magnetic
Highlight:

Gh3039 nickel based superalloy

,

High Strength nickel based superalloy

,

Corrosion Resistant nickel based superalloy

Product Description

GH3039 alloy, a high-performance nickel-based superalloy, excels in demanding environments due to its exceptional mechanical strength, oxidation resistance, and corrosion resistance. Composed primarily of nickel, chromium, cobalt, and iron, GH3039 maintains its integrity and reliability at temperatures up to approximately 1370°C (2498°F). It offers excellent creep and fatigue resistance, crucial for applications in gas turbines, aerospace components, and chemical processing equipment where prolonged exposure to high temperatures and aggressive environments is common. GH3039 alloy's non-magnetic properties and ability to maintain strength over extended service life make it a preferred choice for critical industrial applications requiring high performance and reliability under extreme conditions.

 

Here's a detailed composition table for GH3039 alloy:

Element Composition (%)
Nickel (Ni) 51.0 - 55.0
Chromium (Cr) 19.0 - 22.0
Cobalt (Co) 15.0 - 20.0
Iron (Fe) 5.0 - 9.0
Molybdenum (Mo) 2.5 - 3.5
Titanium (Ti) ≤ 0.70
Aluminum (Al) ≤ 0.60
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 0.50
Silicon (Si) ≤ 0.50
Phosphorus (P) ≤ 0.015
Sulfur (S) ≤ 0.010
Boron (B) ≤ 0.006

GH3039 alloy is primarily composed of nickel, chromium, cobalt, and iron, with minor additions of molybdenum, titanium, aluminum, and trace elements to achieve its desired properties for high-temperature and corrosion-resistant applications.

 

Gh3039 High Strength Corrosion Resistant Nickel-Based Superalloy For Demanding High-Temperature Applications 0

Gh3039 High Strength Corrosion Resistant Nickel-Based Superalloy For Demanding High-Temperature Applications 1

 

Sitemap |  Privacy Policy | China Good Quality Stainless Steel Plate Sheet Supplier. Copyright © 2024-2025 Jiangsu Zhonggongte Metallurgical Technology Co., Ltd. . All Rights Reserved.