| MOQ: | 100KG |
| Price: | Price is negotiated based on the required specifications and quantity |
| Standard Packaging: | Standard export packaging, or packaging as required |
| Delivery Period: | 5-8 working days, depending on the parameters required for negotiation |
| Payment Method: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Capacity: | 5000 tons per month |
GH4169 Alloy
GH4169 is a high-performance nickel-based superalloy specifically designed for excellent strength and stability at elevated temperatures. It is widely used in demanding applications requiring exceptional thermal and oxidative resistance.
Key Features:
GH4169’s combination of high strength, thermal stability, and corrosion resistance makes it an ideal choice for applications requiring reliable performance under severe conditions.
This description emphasizes the key properties and typical uses of GH4169 alloy, highlighting its suitability for high-performance applications.