GH738 Alloy is a nickel-based superalloy with high strength and oxidation resistance

GH738 Alloy is a nickel-based superalloy with high strength and oxidation resistance

MOQ: 100KG
Price: Price is negotiated based on the required specifications and quantity
Standard Packaging: Standard export packaging, or packaging as required
Delivery Period: 5-8 working days, depending on the parameters required for negotiation
Payment Method: Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Capacity: 5000 tons per month
Detail Information
Place of Origin
China
Brand Name
Zhonggong Special Metallurgy
Certification
ISO Certificate
Model Number
GH738 Alloy
Density:
8.19 G/cm³
Melting Point:
1260-1340°C
Tensile Strength:
900-1100 MPa
Yield Strength:
700-850 MPa
Elongation:
20-35%
Hardness:
250-300 HB
Thermal Conductivity:
11.2 W/m·K
Oxidation Resistance:
Excellent
Applications:
Aerospace, Gas Turbines, High-temp. Components
Highlight:

high strength nickel based alloys

,

high strength nickel based superalloy

Product Description

GH738 Alloy is a high-performance, nickel-based superalloy engineered for exceptional mechanical strength and superior oxidation resistance at elevated temperatures. It is commonly used in aerospace and industrial gas turbine applications due to its ability to maintain structural integrity under extreme conditions.

Key Features:

  • Composition: Primarily nickel, with additions of chromium, cobalt, and other elements for enhanced high-temperature stability and strength.
  • Mechanical Properties: Provides high tensile and yield strength, excellent fatigue resistance, and good ductility.
  • Thermal Stability: Retains mechanical properties over a broad temperature range, making it suitable for high-temperature environments.
  • Oxidation Resistance: Exhibits outstanding resistance to oxidation and corrosion, contributing to longer service life in harsh conditions.
  • Applications: Ideal for components such as turbine blades, vanes, and other critical parts in aerospace engines and industrial turbines.

GH738 Alloy’s robust performance characteristics make it a preferred choice for demanding applications where reliability and durability are paramount.

 

Here’s a table detailing the typical chemical composition of GH738 Alloy:

Element Content (%)
Nickel (Ni) 50.0 - 60.0
Chromium (Cr) 20.0 - 25.0
Cobalt (Co) 7.0 - 10.0
Molybdenum (Mo) 3.0 - 5.0
Titanium (Ti) 2.5 - 4.0
Aluminum (Al) 1.5 - 2.5
Iron (Fe) Balance
Carbon (C) ≤ 0.08
Boron (B) ≤ 0.01
Other Elements Traces

This composition provides GH738 Alloy with its high-temperature strength and resistance to oxidation and corrosion.

 