Equal Grades | UNS N10276 NC17D W.Nr.2.4819 NiMo16Cr15W Hastelloyc-276 NS334(China) |
---|---|
Density | 8.9 G/cm3 |
Size | Client's Requirements |
Weldability | Good |
Type | Bar, Plate, Pipe, Etc |
Name | Inconel 617 |
---|---|
Chemical Composition | Ni (50.0-55.0%), Cr (20.0-24.0%), Co (12.0-15.0%), Mo (8.0-10.0%), Al (0.9-1.3%), Ti (0.4-0.6%), C (0.08% Max), Mn (0.5% Max), Si (0.5% Max), S (0.015% Max), P (0.015% Max) |
Tensile Strength | 690 MPa (100 Ksi) |
Yield Strength | 310 MPa (45 Ksi) |
Elongation | 30% (minimum) |
Chemical Composition | Ni (70.0-76.0%), Cr (14.0-17.0%), Fe (6.0-10.0%), Mo (2.8-3.3%), Ti (0.6-1.0%), Al (0.2-0.6%), C (0.08% Max), Mn (1.0% Max), Si (0.5% Max), S (0.015% Max), P (0.015% Max) |
---|---|
Density | 8.38 G/cm³ |
Melting Point | 1290-1350°C |
Tensile Strength | 965 MPa (140 Ksi) |
Yield Strength | 690 MPa (100 Ksi) |
Name | Inconel 600 NS3102 (NS 312) (1Crl 5 Ni75Fe8) H06600 H03102 NCF 600 N06600 NiCr15Fe 2.4816 |
---|---|
Density | 8.4 G/cm³ |
The Alloy | Is A Nickel-chromium-iron Based Solid Solution Strengthened Alloy |
Width | 1500 |
Length | 6000 |
Composition | Nickel-based Superalloy Containing Chromium, Iron, And Nickel |
---|---|
Density | 8.08 G/cm³ |
Melting Point | 1370-1425°C (2498-2597°F) |
Yield Strength (0.2% Offset) | 700-900 MPa (at Room Temperature) |
Elongation | 45-55% |
Name | Inconel 230 |
---|---|
Chemical Composition | Ni (balance), Cr (20.0-24.0%), Co (10.0-15.0%), Mo (0.5-1.5%), Al (0.5-1.5%), Ti (0.3-0.8%), C (0.1% Max), Mn (1.0% Max), Si (0.5% Max), S (0.015% Max), P (0.015% Max) |
Density | 8.4g/cm3 |
Melting Point | 1360-1400°C |
Tensile Strength | 760 MPa (110 Ksi) |
Name | Inconel 751 Alloy |
---|---|
Density | 8.25g/cm3 |
Melting Point | 1300-1350°C |
Tensile Strength | 965 MPa (140 Ksi) |
Yield Strength | 620 MPa (90 Ksi) |
Name | Nickel Inconel 601 Alloy |
---|---|
Chemical Composition | Ni (72.0-78.0%), Cr (21.0-25.0%), Fe (5.0-10.0%), Mn (1.0% Max), Si (0.5% Max), C (0.1% Max), S (0.015% Max), P (0.015% Max) |
Density | 8.08 G/cm³ |
Melting Point | 1400-1450°C |
Tensile Strength | 690 MPa (100 Ksi) |
Name | Inconel 625 Alloy |
---|---|
Chemical Composition | Ni (58.0-63.0%), Cr (20.0-23.0%), Mo (8.0-10.0%), Fe (5.0% Max), Co (1.0% Max), Nb+Ta (3.15-4.15%), Mn (0.5% Max), Si (0.5% Max), C (0.1% Max), S (0.015% Max), P (0.015% Max) |
Density | 8.44 G/cm³ |
Melting Point | 1290-1350°C |
Tensile Strength | 965 MPa (140 Ksi) |
Name | Nickel Inconel 601 Alloy |
---|---|
Chemical Composition | Ni (72.0-78.0%), Cr (21.0-25.0%), Fe (5.0-10.0%), Mn (1.0% Max), Si (0.5% Max), C (0.1% Max), S (0.015% Max), P (0.015% Max) |
Density | 8.08 G/cm³ |
Melting Point | 1400-1450°C |
Tensile Strength | 690 MPa (100 Ksi) |