Name | Nickel Molybdenum Alloy |
---|---|
Density | ~8.89 G/cm³ (0.320 Lb/in³) |
Melting Point | ~1350-1450°C (2460-2640°F) |
Tensile Strength | ~550 MPa (80 Ksi) |
Yield Strength | ~350 MPa (50 Ksi) |
Name | Hastelloy B Alloy |
---|---|
Density | ~8.89 G/cm³ (0.321 Lb/in³) |
Melting Point | ~1300-1400°C (2370-2550°F) |
Tensile Strength | ~550 MPa (80 Ksi) |
Yield Strength | ~350 MPa (50 Ksi) |
Density | 8.1 G/cm³ |
---|---|
Alloy Type | Nickel-based Alloys |
Melting Point | 1320°C-1390°C |
Thermal Expansion Coefficient | 13.5×10-6 M/mK |
Thermal Coefficient | 11 W/(m·K) |
Name | Nickel Chromium Molybdenum Alloy 59 |
---|---|
Composition | Nickel (approx. 59%), Chromium (approx. 23%), Molybdenum (approx. 16%), Iron (≤ 1%), Copper (≤ 1%), Cobalt (≤ 0.5%), Tungsten (≤ 0.5%), Carbon (≤ 0.01%), Silicon (≤ 0.1%), Phosphorus (≤ 0.02%) |
Key Features | Excellent Corrosion Resistance In Highly Acidic Environments, High Strength, Good Weldability |
Applications | Chemical Processing, Petrochemical Industry, Pollution Control, Desalination |
Strength | High Mechanical Strength And Toughness |
Name | Nickel Based Alloys |
---|---|
Composition | Nickel (31.5-32.5%), Chromium (26-27%), Molybdenum (6-7%), Iron (Bal.), Nitrogen (≤0.15%), Copper (≤1.4%), Carbon (≤0.015%) |
Key Features | Excellent Resistance To Corrosion In Aggressive Media, High Strength |
Applications | Chemical Processing, Pulp And Paper Industry, Flue Gas Desulfurization |
Strength | High Mechanical Strength And Resistance To Crevice Corrosion |
Name | Nickel Based Alloys |
---|---|
Alloy Type | Nickel-Chromium Superalloy |
Density | ~8.42 G/cm³ (0.305 Lb/in³) |
Melting Point | ~1360-1410°C (2480-2570°F) |
Tensile Strength | ~1100 MPa (160 Ksi) |
Tensile Strength | Approximately 800-950 MPa |
---|---|
Yield Strength | ≥500 MPa |
Elongation | ≥30% |
Density | Approximately 8.0 G/cm³ |
Hardness | Typically Rockwell C 30-40 |
Tensile Strength | Approximately 800-950 MPa |
---|---|
Yield Strength | ≥500 MPa |
Elongation | ≥30% |
Density | Approximately 8.0 G/cm³ |
Hardness | Typically Rockwell C 30-40 |
Density | 8.24 G/cm³ |
---|---|
Alloy | Nickel-based High-temperature Alloys |
High Temperature Strength | Excellent |
Corrosion Resistance | Excellent |
Ease Of Processing | Excellent |
Name | Inconel 625 Alloy |
---|---|
Chemical Composition | Ni (58.0-63.0%), Cr (20.0-23.0%), Mo (8.0-10.0%), Fe (5.0% Max), Co (1.0% Max), Nb+Ta (3.15-4.15%), Mn (0.5% Max), Si (0.5% Max), C (0.1% Max), S (0.015% Max), P (0.015% Max) |
Density | 8.44 G/cm³ |
Melting Point | 1290-1350°C |
Tensile Strength | 965 MPa (140 Ksi) |