Density | 8.1 G/cm³ |
---|---|
Alloy Type | Nickel-based Alloys |
Melting Point | 1320°C-1390°C |
Thermal Expansion Coefficient | 13.5×10-6 M/mK |
Thermal Coefficient | 11 W/(m·K) |
Composition | Titanium Alloy With Primarily Titanium And Additional Elements (exact Composition Varies). |
---|---|
Tensile Strength | High Tensile Strength, Suitable For High-stress Applications. |
Yield Strength | Excellent Yield Strength, Providing Reliability Under Load. |
Corrosion Resistance | Outstanding Resistance To Corrosion, Including In Marine And Chemical Environments. |
Fatigue Resistance | High Fatigue Strength, Minimizing The Risk Of Failure Under Cyclic Loading. |
Name | Nickel Based Alloy 75 Ti-6Al-4V |
---|---|
Composition | Titanium (Ti), 6% Aluminum (Al), 4% Vanadium (V) |
Density | 4.43g/Cm3 |
Tensile Strength | 1050 MPa (at Room Temperature) |
Yield Strength | 950 MPa (at Room Temperature) |
Name | High Strength Titanium TB2 Alloy |
---|---|
Density | 4.43 G/cm³ |
Tensile Strength | 1,200 MPa |
Yield Strength | 1,100 MPa |
Elongation | 12% |
Name | Nickel Based Alloy HC-4 |
---|---|
Composition | Nickel-based Alloy With High Nickel, Chromium, And Iron Content |
Strength | Exceptionally Strong, Suitable For High-stress Applications |
High-Temperature Stability | Maintains Integrity At Elevated Temperatures |
Corrosion Resistance | Highly Resistant To Corrosion And Oxidation |
Density | 8.24 G/cm³ |
---|---|
Alloy | Nickel-based High-temperature Alloys |
High Temperature Strength | Excellent |
Corrosion Resistance | Excellent |
Ease Of Processing | Excellent |
Pricing Of Goods | According To Actual Weight |
---|---|
Processing Services | Bending, Cutting, Unwinding, Forming, Stamping, Welding |
The Density Range Is | 8.19 To 8.24 G/cm ³ |
Inconel 718 | Is A Nickel Based High-temperature Alloy |
Melting Point | 1260-1340°C |
Name | Incoloy Alloy 800H |
---|---|
Density | 8.0-8.2 G/cm³ |
Melting Point | 1350-1400°C (2460-2550°F) |
Tensile Strength | 520-690 MPa (75,400-100,000 Psi) |
Yield Strength (0.2% Offset) | 205-310 MPa (29,700-45,000 Psi) |
Name | Nickel Based Alloys |
---|---|
Alloy Type | Nickel-Chromium Superalloy |
Density | ~8.42 G/cm³ (0.305 Lb/in³) |
Melting Point | ~1360-1410°C (2480-2570°F) |
Tensile Strength | ~1100 MPa (160 Ksi) |
Name | Titanium Hollow Tube |
---|---|
Density | 4.51 G/cm³ |
Tensile Strength | Approx. 240 MPa |
Yield Strength | Approx. 170 MPa |
Elongation | 24% |