Name | Incoloy 925 Alloy |
---|---|
Density | 8.14g/cm3 |
Melting Point | Approximately 1310-1350°C (2390-2460°F) |
Tensile Strength | 870-1100 MPa (126,000-160,000 Psi) |
Yield Strength (0.2% Offset) | 690-965 MPa (100,000-140,000 Psi) |
Packaging Details | Standard export packaging, or packaging as required |
---|---|
Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Ability | 5000 tons per month |
Place of Origin | China |
Name | Incoloy Alloy 825 |
---|---|
Density | 8.14g/Cm3 |
Melting Point | 1370-1400°C (2498-2552°F) |
Tensile Strength | 550-690 MPa (79,800-100,000 Psi) |
Yield Strength (0.2% Offset) | 240-345 MPa (34,800-50,000 Psi) |
Density | 8.3 G/cm³ |
---|---|
Melting Point | 1300-1400°C |
Tensile Strength | 900-1200 MPa |
Yield Strength | 700-950 MPa |
Elongation | 15-30% |
Density | 8.89 G/cm³ |
---|---|
Delivery Status | Black Or Bright |
Process | Cutting Forging Hot Rolling Cold Rolling |
Processing Services | Can Be Deep Processed, Welded, Polished |
Heat Treatment | Solution Aging, Quenching And Tempering, Heat Treatment |
Density | 8.75 G/cm³ |
---|---|
Melting Point Is About | 1300-1350°c |
Tensile Strength Up To | 650 MPa |
Width | 1000mm 1219mm 1500mm Or As Required |
Services | Cutting, Bending |
Chemical Composition | Ni (70.0-76.0%), Cr (14.0-17.0%), Fe (6.0-10.0%), Mo (2.8-3.3%), Ti (0.6-1.0%), Al (0.2-0.6%), C (0.08% Max), Mn (1.0% Max), Si (0.5% Max), S (0.015% Max), P (0.015% Max) |
---|---|
Density | 8.38 G/cm³ |
Melting Point | 1290-1350°C |
Tensile Strength | 965 MPa (140 Ksi) |
Yield Strength | 690 MPa (100 Ksi) |
Composition | Nickel-based Superalloy Containing Nickel, Chromium, Molybdenum, And Niobium |
---|---|
Density | 8.4 G/cm³ |
Melting Point | 1290-1350°C (2354-2462°F) |
Tensile Strength | 760-1035 MPa (at Room Temperature) |
Yield Strength (0.2% Offset) | 350-765 MPa |
Packaging Details | Standard export packaging, or packaging as required |
---|---|
Delivery Time | 5-8 working days, depending on the parameters required for negotiation |
Payment Terms | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
Supply Ability | 5000 tons per month |
Place of Origin | China |
Density | 8.9 G/cm³ |
---|---|
Tensile Strength | 950 - 1250 MPa |
Yield Strength | 500 - 750 MPa |
Elongation | 20-35% |
Melting Point | 1300 - 1370°C |