Density | 8.2 G/cm³ |
---|---|
Tensile Strength | 900 - 1250 MPa |
Yield Strength | 450 - 750 MPa |
Elongation | 18 - 28% |
Thermal Conductivity | 1370 - 1420°C |
Density | 8.3 G/cm³ |
---|---|
Tensile Strength | 1000 - 1300 MPa |
Yield Strength | 500 - 800 MPa |
Elongation | 15 - 25% |
Thermal Conductivity | 1350 - 1450°C |
Density | 8.4 G/cm³ |
---|---|
Tensile Strength | 1000 - 1300 MPa |
Yield Strength | 500 - 800 MPa |
Elongation | 15 - 25% |
Thermal Conductivity | 1350 - 1450°C |
Composition | Nickel-based Superalloy Containing Chromium, Iron, And Nickel |
---|---|
Density | 8.08 G/cm³ |
Melting Point | 1370-1425°C (2498-2597°F) |
Yield Strength (0.2% Offset) | 700-900 MPa (at Room Temperature) |
Elongation | 45-55% |
Density | ~8.35 G/cm³ (0.302 Lb/in³) |
---|---|
Melting Point | ~1300-1400°C (2370-2550°F) |
Tensile Strength | ~900 MPa (130 Ksi) |
Yield Strength | ~700 MPa (102 Ksi) |
Elongation | ~20% |
Density | ~8.8 G/cm³ (0.317 Lb/in³) |
---|---|
Melting Point | ~1300-1400°C (2370-2550°F) |
Tensile Strength | ~900 MPa (130 Ksi) |
Yield Strength | ~700 MPa (102 Ksi) |
Elongation | ~15% |
Density | ~8.9 G/cm³ (0.321 Lb/in³) |
---|---|
Melting Point | ~1350-1450°C (2460-2640°F) |
Tensile Strength | ~850 MPa (123 Ksi) |
Yield Strength | ~700 MPa (102 Ksi) |
Elongation | ~15% |
Density | ~8.9g/cm³ (0.321 Lb/in³) |
---|---|
Melting Point | ~1350-1450°C (2460-2640°F) |
Tensile Strength | ~900 MPa (130 Ksi) |
Yield Strength | ~750 MPa (109 Ksi) |
Elongation | ~15% |
Density | ~8.8 G/cm³ (0.317 Lb/in³) |
---|---|
Melting Point | ~1350-1450°C (2460-2640°F) |
Tensile Strength | ~950 MPa (138 Ksi) |
Yield Strength | ~800 MPa (116 Ksi) |
Elongation | ~15% |
Density | 8.19 G/cm³ |
---|---|
Melting Point | 1260-1340°C |
Tensile Strength | 900-1100 MPa |
Yield Strength | 700-850 MPa |
Elongation | 20-35% |